Molding success for you!

Product Detail
12cavities Jar PET preform mould

12cavities Jar PET preform mould

Yige Mold 12 Cavities Jar PET Preform Mould—CNC precision-machined with high-hardness steel for heavy-duty jar preform production. Ultra-tight tolerance, anti-wear structure, fast injection cycles, engineered for non-stop industrial packaging manufacturing worldwide.
Detail
Mould Name 12cavities Jar PET preform mould Mould Main Materia S420,2316,2083
Mould Cavity 12Cavity Delivery Time 35-45working days

Technical Analysis of 12-Cavity Wide-Mouth Jar PET Preform Mold


I. Mold Architecture and Engineering Logic

The 12-cavity wide-mouth jar PET preform mold is a cluster injection system designed for ultra-large-scale industrial production, employing a three-tier modular architecture: base frame layer, hot runner integration layer, and cavity unit layer. The mold adopts a dual-layer circular array layout (6 cavities on the upper layer + 6 cavities on the lower layer), ensuring equal melt flow paths through a central radial runner topology. Each cavity is independently equipped with a four-point guide pillar positioning system, coupled with a conical clamping mechanism with a precision of 0.02mm, achieving mold clamping parallelism error ≤ 0.05mm.


II. Breakthroughs in Flow Field Dynamics Design

The gating system features a three-stage pressure attenuation structure: the primary runner uses a Φ28mm variable cross-section design, the secondary runner employs hyperbolic transition surfaces, and the tertiary gate zone incorporates a Venturi effect acceleration section. The hot runner is equipped with zoned temperature control compensation modules, dividing the 12 hot nozzles into four independently controlled temperature groups. Through embedded thermocouples for real-time monitoring, melt temperature differences at each cavity inlet are maintained ≤ ±1.8°C. To address the large cross-section of wide-mouth preforms, an innovative spiral-expanding flow guide cavity is designed in the gate area, reducing the transition length from the Φ6mm gate to the Φ48mm cavity by 40%.


III. Thermodynamic Management System Reconfiguration

The cooling system implements a three-dimensional network layout: axially arranged in 12 annular water channels (layer spacing: 8mm), radially configured with 36 sets of tapered cooling pin arrays (pin diameter: Φ3mm/Φ5mm gradient), forming an isothermal gradient control field. A proprietary zoned counterflow cooling technology is employed: the upper six cavities use 20→10°C reverse-temperature cooling, while the lower six cavities use 15→25°C forward-temperature cooling, eliminating mold thermal deformation through temperature difference offset. High thermal conductivity beryllium-copper alloy inserts are embedded in key thermally sensitive areas (neck threads, transition arcs), improving thermal conductivity efficiency by 300% compared to standard steel.


IV. Materials Science and Surface Engineering

The mold core utilizes dual-layer composite steel: the base material is German 1.2344 ESR electroslag remelted steel, with a 2mm thick cobalt-based alloy layer (Co-Cr-Mo-W) surface cladding. After undergoing a three-stage heat treatment process—1020°C vacuum quenching → -120°C cryogenic treatment → 560°C triple tempering—a gradient match is achieved with surface hardness HRC 54–56 and core toughness HRC 46–48. The runner system employs physical vapor deposition technology, depositing a 3μm thick TiAlN nano-coating on the runner walls, reducing the friction coefficient to 0.15 and improving anti-adhesion performance by 5 times.


V. Precision Manufacturing and Assembly System

Cavity machining adopts a seven-step composite process: high-speed milling (0.3mm allowance) → deep-hole drilling (water channel machining) → EDM forming (detailed features) → slow wire cutting (precision contours) → ultrasonic vibration polishing (Ra 0.025μm) → plasma electrolytic oxidation (surface hardening) → laser micro-texturing (demolding texture). The assembly process implements four-level precision control: base plate flatness ≤ 0.01mm/m → guide pillar perpendicularity ≤ 0.005mm → cavity positional tolerance ≤ 0.015mm → hot nozzle coaxiality ≤ 0.02mm.


VI. Production Verification and Quality Control

A full lifecycle testing protocol is established:

  1. Hydrodynamic Verification: Fill testing using red tracer, cavity fill time difference ≤ 0.15 seconds


  2. Thermal Imaging Calibration: Infrared thermography monitoring, cavity surface temperature difference ≤ 2.5°C


  3. Continuous Production Testing: 120-hour uninterrupted operation, recording key parameters:


Monitoring Indicator

Standard Requirement

Measured Data

Single Cavity Weight Variation

≤ ±0.45%

0.28%–0.32%

Neck Ovality

≤ 0.04mm

0.022–0.031mm

Wall Thickness Uniformity

Range ≤ 0.25mm

0.12–0.18mm

Crystallinity Distribution

32 ± 3%

31.5%–33.8%

Cycle Time Stability

σ ≤ 0.8 seconds

σ = 0.62 seconds


VII. Special Application Adaptation Solutions

  1. High-Pressure Packaging Preforms: An annular stress diffusion rib is added to the shoulder area. After finite element analysis optimization, burst pressure increases from 2.8MPa to 3.6MPa.


  2. Light-Blocking Packaging Solution: Through micro-prism structure design on the mold surface (prism height: 15μm, spacing: 30μm), preform light transmittance is reduced from 92% to 35%.


  3. Advanced Lightweighting: Using an asymmetric wall thickness algorithm, non-load-bearing areas of the preform body are thinned to 1.6mm, achieving an 18% overall weight reduction while passing a 1.5m drop test.



VIII. Maintenance Engineering System

A predictive maintenance framework is designed:

  1. Wear Monitoring: Acoustic emission sensors installed on ejector pins and sliders provide early warning of abnormal wear 3,000 cycles in advance through spectrum analysis.


  2. Corrosion Protection: Magnesium alloy sacrificial anodes are installed in cooling channels, coupled with real-time pH monitoring.


  3. Rapid Repair: An in-situ laser cladding repair process is developed, capable of repairing damage up to 0.5mm deep without mold disassembly.



IX. Energy Efficiency and Economics

  • Production Cycle: 33% faster than 8-cavity molds, with an 18% reduction in energy consumption per ton of product.


  • Mold Lifespan: Up to 3.5 million cycles with routine maintenance; key wear components (hot nozzles, ejector pins) feature quick-change designs.


  • Investment Recovery: Payback period ≤ 16 months at an annual production scale of 15 million units.



YIGE MOLD factory

Email: quotaiton@yigemold.com  Tel & Whatsapp : +86 15867628215

Hi
 
 
 
 
 Work Time
Mon to Fri :8:00-21:00
Sat to Sun :9:00-17:00
 Contact Details
Mob/Whatsapp:0086 15867628215
Email:quotation@yigemold.com